Coating Electrodes
-

WTC-90
-

TC-02
-

CC-01
-

TB-01
-

ZB-01
| Code No. | Name | Applicable | Maximum Hardness (HMV) |
|---|---|---|---|
| WTC-90 | Tungsten-Carbide | SK, SKH, SKA, SKD-11,
SKD-61, S50C, SUS and other steels |
2,000 |
| TC-02 | Titanium Carbide | 3,200 | |
| CC-01 | Chromium Carbide | 1,800 | |
| VC-01 | Vanadium Carbide | 2,300 | |
| TB-01 | Titanium Boride | 2,600 | |
| ZB-01 | Zirconia Boride | 2,200 | |
| CMC-01 | Cobalt, Molybdenum, Chromium | 600 | |
| MO-01 | Molybdenum | 280 | |
| W-01 | Tungsten | 330 |
Overlay Electrodes
-

SD-01
-

SD-11
-

SD-21
-

AL-02
-

CU-02
| Code No. | Applicable | Hardness (HRC) | Application |
|---|---|---|---|
| SD-01 | SKD, NAK, HPM, PDS, SCM, STAVAX, S50, SC, FC, FCD, SUS, and other steels, Beryllium Copper, Ni Electrocasting, etc. |
35 | ・Parting Lines Overlay repairing for plastic injection molds occurred burrs on productions ・ Diecasting dies Overlay repairing at erosion parts ・ Rolls, Rams, Shafts etc. Overlay repairing |
| SD-11 | 51 | ・ Hardened steel Overlay repairing ・ Stellite welding underfill, distortion, pin-holes Overlay repairing |
|
| SD-21 | 60 | ・ Hardened steel Overlay repairing ・ Overlay requiring texturing, chrome plating, or plating |
|
| AL-02 | Al Alloy | - | ・ Al alloy molds Overlay repairing ・ Al Wheel porosity Overlay repairing ・ Al Diecasting products porosity Overlay repairing |
| CU-02 | Cu Alloy | - | ・ BeCu molds Overlay repairing ・ Cu molds Overlay repairing by Cu alloy |
Applicators
| Model | Standard |
Miniature |
Vibrating
|
|
|---|---|---|---|---|
| Dimension | Max dia. (mm) | 91 | 48 | 48 |
| Length (mm) | 302 | 224 | 206 | |
| Weight (Kg) | 2.6 | 1 | 0.8 | |
| Electrode Motions | Rotation 1 to 1,050 rpm |
Rotation 2,000 to 8,000 rpm |
Vibration (forward-backward) 3,000 / min (50Hz) 3,600 / min (60Hz) |
|
| Electrode Size (mm) | dia. 1 to 10 | dia. 1 to 4 | dia. 1 to 3 1 × 3 (Flat) 2 × 2 (Square) etc. |
|
| Application | Coating | ✓ | ✓ | ✓ |
| Overlay | ✓ | ✓ | × | |
| Grinding | × | ✓ | × | |